| Product name | PAKUNA ELECTOR CX |
| Usage | |
| Standard process condition | Concentration 60-140g/L Temperature 30-60℃ Time 1-2 minutes (rack) 3-10 minutes (barrel) Polarization anode |
| Advantage | ◆Cost reduction by prolonging product’s life span ◆ Low inhibition due to sedimentation of heavy metal and low COD reduce burden of wastewater treatment. ◆ Due to excellent property of removing smuts, finished surface of plating is good. ◆ Suitable to ferrous materials. |