HOME > Product Search > Product Details

| Product name | METASU FZ-77M1/GR1 |
| Usage | |
| Standard process condition | Zinc chloride 30-60g/L Metal Zinc 15- 30g/L Total chlorine 120-160g/L Total chloride 180-220g/L (total amount of potassium chloride and ammonium chloride) Ammonium chloride 30g/L or more METASU FZ-77M1 30mL/L METASU FZ-77GR1 0.5-3mL/L pH 5.2-6.0 Bath temperature 20-60℃ |
| Advantage | ◆Applicable to wide-range bath temperature. ◆Excellent and high bright plating films from ambient to high bath temperature is obtainable. ※Especially, at high bath temperature, the following advantages can be obtained. ① Bath does not need to be cooled down. ② The surface level does not increase. ③ Physical properties of plating film improve with superior secondary workability and prevent it from chipping. ④ Adhesive property of chromate is improved. ◆Low mist and odor provides better working environment. |
| Product name | MSDS Download |
| METASU FZ-77M1 | |
| METASU FZ-77GR1 | |
| {$=detail_name3} | |
| {$=detail_name4} | |
| {$=detail_name5} |
|
|